Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 150 g/m² | >= 93.8 lb/ream | |
ArcelorMittal AS150 Aluminized steel Applications: Alusi® coating is resistant to heat, high temperature oxidation and corrosion, and offers a high level of reflectivity, making it suitable for applications in a corrosive atmosphere .. |