Polymer Property : Coating Weight = 156 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 250 g/m²
156 lb/ream
entire thickness; NF EN ISO 2286.2
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Coating Weight 250 g/m²
156 lb/ream
entire thickness; NF EN ISO 2286.2
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.