Coating Weight 35.7 g/m²
22.3 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 40LL539 OPP Film
Product Description: A clear, two-side coated, polypropylene label facestock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are required..
Coating Weight 35.7 g/m²
22.3 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 50LH247 OPP Film
Product Description: A super white opaque, cavitated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. 50LH247 also shows excellent performances on reel..
Coating Weight 35.7 g/m²
22.3 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 50MH247 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial..