Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 225 g/m² | >= 141 lb/ream | double-sided |
ArcelorMittal Extragal® Z225 Double-sided pure zinc galvanized steel Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib.. |