Physical Properties Metric English Comments
Coating Weight 27.7 g/m²
17.3 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 30MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s..
Coating Weight 27.7 g/m²
17.3 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 30LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
Coating Weight 27.7 g/m²
17.3 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 30MBT666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r..