Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 64.6 g/m² | >= 40.4 lb/ream | 520 |
ExxonMobil Label-Lyte® 95 LBM-301 White Opaque OPP Film for Blow Mold Label Applications White, one-side treated polypropylene label designed for blow mold label applications. As the label becomes part of the container, the result is a "direct print" look. This film satisfies the demand.. |