Polymer Property : Coating Weight = 55.0 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 30.0 - 55.0 g/m²
18.8 - 34.4 lb/ream
ArcelorMittal ZF90 Galvannealed zinc-iron alloy coated steel
Applications: The excellent corrosion protection and high surface quality offered by Galvannealed coatings make these products well suited for numerous automotive applications involving both visible..