Coating Weight 949 g/m²
593 lb/ream
Ten Percent
Mid-Mountain Materials ARMATEX® SRS 28 Silica Fabric Coated with Silicone Rubber
ARMATEX® SRS 28 is a silica fabric coated with silicone rubber on one or both sides to a finished weight of 28 oz/sq yd. An ideal product for heavy duty protection of equipment and personnel, ARM..