Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM ISO 100 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM ISO 220 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM ISO 32 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM ISO 46 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM ISO 68 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Oxidative Stability | >= 15000 hour | >= 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco FM Seamer Oil FeaturesChevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications... |
|||
Oxidative Stability | 15000 hour | 15000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco GST® EP ISO 32 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |