Oxidative Stability >= 24000 hour
>= 24000 hour
TOST, (modified),; ASTM D943-04a
ConocoPhillips Hydroclear Diamond Class® 32 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
Oxidative Stability >= 24000 hour
>= 24000 hour
TOST; ASTM D943-04a
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
Oxidative Stability >= 24000 hour
>= 24000 hour
TOST; ASTM D943-04a
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..