Physical Properties | Metric | English | Comments |
---|---|---|---|
a Lattice Constant | 3.79 Ã… | 3.79 Ã… | |
MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
a Lattice Constant | 3.79 Ã… | 3.79 Ã… | |
Mateck Lanthanum Aluminate Substrate, LaAlO3 cubic Substrate single crystals for superconductivity |
|||
a Lattice Constant | 3.79 Ã… | 3.79 Ã… | |
Mateck Lanthanum Aluminate Substrate, LaAlO3 rhombohedral Substrate single crystals for superconductivity |