Polymer Property : a Lattice Constant = 5.4093 Ã…
Polymer Property :
a Lattice Constant =
5.4093 Ã…
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
a Lattice Constant
5.4093
Ã…
5.4093
Ã…
Mateck Zinc Sulphide, ZnS
Semiconductor single crystals. Twins and stacking faults < 4% of hexagonal phase.