Polymer Property : Linear Mold Shrinkage, Transverse = 0.0022 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific)
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific)
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON RV00AES PA 66
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00AES PA 66
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON RX06422 PA 66
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX06422 PA 66
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific)
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific)
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.