Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC
LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific)
LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC
LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific)
LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact.