Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0031 - 0.0037 cm/cm @Time 86400 sec |
0.0031 - 0.0037 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |