Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DFI12E PC
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubriloy D20001 PC
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by..
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Transverse 0.0057 cm/cm

@Time 86400 sec
0.0057 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.