Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0051 - 0.0058 cm/cm

@Time 86400 sec
0.0051 - 0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Linear Mold Shrinkage, Transverse 0.0051 - 0.0058 cm/cm

@Time 86400 sec
0.0051 - 0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific)
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.