Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0068 cm/cm @Time 86400 sec |
0.0068 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific) LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0068 - 0.0078 cm/cm @Time 86400 sec |
0.0068 - 0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.0068 - 0.0078 cm/cm @Time 86400 sec |
0.0068 - 0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0068 cm/cm @Time 86400 sec |
0.0068 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |