Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0069 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC
LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing 20% Milled Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific)
LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp DF0069E PC
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific)
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES
LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific)
LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF006LZZ PES
LNP THERMOCOMP* JF006LZZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Extrusion Grade, Low Extractable.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific)
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based ..
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Time 86400 sec
0.0069 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard..