Linear Mold Shrinkage, Transverse 0.0151 - 0.0167 cm/cm

@Time 86400 sec
0.0151 - 0.0167 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP COLORCOMP M1000S PP
LNP COLORCOMP* M1000S is an unfilled Polypropylene resin. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0151 cm/cm

@Time 86400 sec
0.0151 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.