Linear Mold Shrinkage, Transverse 0.021 - 0.029 cm/cm

@Time 86400 sec
0.021 - 0.029 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.