Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 0.39 cSt | 0.39 cSt | Liquid |
3M Novec™ 612 Magnesium Protection Fluid Novec 612 fluid, dodecafluoro-2-methyl-3-pentanone or (CF3CF2C(O)CF(CF3)2, is a clear, colorless, and low odor fluid. Its properties, environmental profile, and margin of safety make it a sustainabl.. |