Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 0.78 cSt | 0.78 cSt | kinetic/kinematic |
Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP Non Ozone depleting, VOC exempt, Silicone cleaner to clean Plastic and Metals, excellent for removing oils, silicone-based car wax and protectants.Information provided by Dow Corning |