Polymer Property : Viscosity Measure = 14 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 84 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 56 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Viscosity Measure 14 cSt

@Temperature 25.0 °C
14 cSt

@Temperature 77.0 °F
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow