Physical Properties Metric English Comments
Viscosity Measure 15.5 cSt
15.5 cSt
Toluene Solution; Finaprene 1008 Test
Total Finaprene® 503 Styrene-Butadiene TPE Copolymer  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 503 is a thermoplastic elastomer type linear butadiene-butadiene block copolymer (SBS). Thanks to its high styrene content, Finaprene® 503 provi..