Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 19.5 cSt | 19.5 cSt | Toluene Solution; Finaprene 1008 Test |
Total Finaprene® 409 Styrene-Butadiene TPE Copolymer
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 409 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Because of its high molecular weight, Finaprene® 409 provi.. |