Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 2.4 cSt | 2.4 cSt | Kinetic/Kinematic |
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room.. |