Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 32 cSt @Temperature 40.0 °C |
32 cSt @Temperature 104 °F |
ASTM D445, DIN 51 361 |
Chesterton 390 Cutting Oil Description: Chesterton® 390 Cutting Oil is a heavy duty, multi-purpose cutting fluid designed to provide maximum tool life and superior parts finish in severe applications. It is a highly reinforc.. |