Physical Properties Metric English Comments
Viscosity Measure 300 - 360 cSt

@Temperature 25.0 °C
300 - 360 cSt

@Temperature 77.0 °F
ASTM D445-94
Dow VORANOL™ CP 450 Polyol
VORANOL™ CP 450 polyol is a glycerine propoxylated polyether triol.Information provided by Dow