Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 50000 cSt | 50000 cSt | Kinetic/Kinematic |
Dow Corning 3-0134 Polymer 50,000 CS Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity= 50,000 cp.Information provided by Dow Corning |