Physical Properties Metric English Comments
Viscosity Measure 7.0 cSt
7.0 cSt
5.23% Toluene solution; NM-300-11
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS)
Solprene 4302 is a linear block copolymer of styrene and butadiene, having 31% styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non..
Viscosity Measure 7.0 cSt
7.0 cSt
Toluene solution viscosity 5,23%; NM 300-11
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry
Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a ..