Physical Properties Metric English Comments
Viscosity Measure 600 - 700 cSt

@Temperature 37.8 °C
600 - 700 cSt

@Temperature 100 °F
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt..