Physical Properties Metric English Comments
Viscosity Measure 6.0 - 8.0 cSt

@Temperature 100 °C
6.0 - 8.0 cSt

@Temperature 212 °F
Unipetrol Middle Oil Hydrogenate
Oil hydrogenates are a fraction boiling at above approximately 300°C, gained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of semi-soli..