Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 870 cSt @Temperature 25.0 °C |
870 cSt @Temperature 77.0 °F |
|
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |