Polymer Property : Spiral Flow = 106 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 106 - 106 cm

@Temperature 250 - 250 °C
41.7 - 41.7 in

@Temperature 482 - 482 °F
Average value: 106 cm Grade Count:1
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Spiral Flow 106 - 106 cm

@Thickness 2.00 - 2.00 mm
41.7 - 41.7 in

@Thickness 0.0787 - 0.0787 in
Average value: 106 cm Grade Count:1
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..