Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 30.0 cm @Thickness 1.00 mm |
11.8 in @Thickness 0.0394 in |
SABIC Method |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Spiral Flow | 30.0 cm @Thickness 1.00 mm |
11.8 in @Thickness 0.0394 in |
SABIC Method |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Spiral Flow | 30.0 cm @Thickness 1.50 mm, Temperature 80.0 °C |
11.8 in @Thickness 0.0591 in, Temperature 176 °F |
290/1000 Bar |
BASF Ultramid® A3EG10 High Speed Information provided by BASF |
|||
Spiral Flow | 30.0 cm @Thickness 1.00 mm |
11.8 in @Thickness 0.0394 in |
SABIC Method |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |