Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120 PPE
Noryl* SA120 resin is a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120 is intended for use as additive or building block in a variety of thermoplastics, thermoplastic..
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120 PPE (Asia Pacific)
Noryl* SA120 resin is a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120 is intended for use as additive or building block in a variety of thermoplastics, thermoplastic..
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120 PPE (Europe-Africa-Middle East)
Noryl* SA120 resin is a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120 is intended for use as additive or building block in a variety of thermoplastics, thermoplastic..
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120FIN PPE
Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the..
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120FIN PPE (Asia Pacific)
Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the..
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL SA120FIN PPE (Europe-Africa-Middle East)
Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the..