Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.00670 g/cc | 0.000242 lb/in³ | After expansion |
Sekisui PIOCELAN OP-15D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |