Polymer Property : Bulk Density = 0.000939 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0220 - 0.0260 g/cc
0.000795 - 0.000939 lb/in³
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Bulk Density 0.0220 - 0.0260 g/cc
0.000795 - 0.000939 lb/in³
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Bulk Density 0.0220 - 0.0260 g/cc
0.000795 - 0.000939 lb/in³
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Bulk Density 0.0220 - 0.0260 g/cc
0.000795 - 0.000939 lb/in³
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..