Bulk Density 0.0601 - 0.128 g/cc
0.00217 - 0.00463 lb/in³
As Produced
Skamol Group Exfoliated/Loose Vermiculite Loose Vermiculite
SKAMOL exfoliated vermiculite has the following characteristics: Max. service temperature: Up to 1200°C (2192°F)Good thermal insulating propertiesLow densityLow heat capacityAbsorbing and free..
Bulk Density 0.0600 g/cc
0.00217 lb/in³
Scott
TIMCAL TIMREX® PG10 Natural P/M Special-Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..