Polymer Property : Bulk Density = 0.00686 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.100 - 0.190 g/cc
0.00361 - 0.00686 lb/in³
Packed Density
Zircar Ceramics ALBF Alumina Bulk Fiber
Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give ..
Bulk Density 0.100 - 0.190 g/cc
0.00361 - 0.00686 lb/in³
Packed Density
Zircar Ceramics ALBF-1 Alumina Bulk Fiber
Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo..