Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | Loose |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | Loose |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.220 - 0.420 g/cc | 0.00795 - 0.0152 lb/in³ | |
Pau Tai UNINOX PA-401 PVC Processing Aid UNINOX PA-401 is a high molecular weight MMSAN (methyl methacrylate-styrene-acrylonitrile) processing aid. It is a cost effective processing aid for rigid PVC compounds such as calendered sheet, ext.. |
|||
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 P350 PUT Pelletized Carbon Fiber, Polyurethane Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Bulk Density | 0.220 g/cc | 0.00795 lb/in³ | Loose |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.220 - 0.420 g/cc | 0.00795 - 0.0152 lb/in³ | |
Pau Tai UNINOX PA-551 PVC Processing Aid UNINOX PA-551 is a high molecular weight acrylic polymer resin. This processing aid contributes greatly to rapid growth markets for rigid or flexible PVC compounds such as calendered sheet, extrusio.. |