Bulk Density 0.192 - 0.240 g/cc
0.00694 - 0.00868 lb/in³
Loose
KaMin KaMin® 90 Kaolin clay - Waterwashed
KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati..
Bulk Density 0.192 - 0.240 g/cc
0.00694 - 0.00868 lb/in³
Loose
KaMin Polyfil® F Kaolin Clay - Waterwashed
Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water ..