Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.2403 g/cc | 0.008681 lb/in³ | |
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Bulk Density | 0.2403 g/cc | 0.008681 lb/in³ | |
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Bulk Density | 0.2403 g/cc | 0.008681 lb/in³ | |
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Bulk Density | 0.2403 g/cc | 0.008681 lb/in³ | |
Zircar Zirconia ZYF-50 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |