Polymer Property : Bulk Density = 0.00937 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.260 g/cc
0.00937 lb/in³
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Bulk Density 0.260 g/cc
0.00937 lb/in³
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Bulk Density 0.260 g/cc
0.00937 lb/in³
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.