Physical Properties Metric English Comments
Bulk Density >= 0.0100 g/cc
>= 0.000361 lb/in³
Typical
SYNTHOS Koplen® 1640 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor..