Polymer Property : Bulk Density = 0.0104 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.288 g/cc
0.0104 lb/in³
Dry
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Loose
CIMBAR CLEAR-BLOC® 80 Antiblock Talc
CLEAR-BLOC® 80 talc, produced from high purity ore provides high brightness, clarity, low iron content and low surface area for primary use as an anti-block additive in LDPE and LLDPE film applicat..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder
Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 711 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 721 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 741 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® LBG1 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® HSV Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 201 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 2801-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Bulk Density 0.288 g/cc
0.0104 lb/in³
Arkema Group KYNAR® 761 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..