Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 134 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons ECORAX® 1720 Carbon Black Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | ISO 60 |
SABIC PVC 673E Emulsion Polyvinyl Chloride Product Description: PVC 673E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosi.. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | ISO 60 |
SABIC PVC 701E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 701E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosi.. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | ISO 60 |
SABIC PVC 703E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 703E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosi.. |
|||
Bulk Density | 0.320 - 0.480 g/cc | 0.0116 - 0.0173 lb/in³ | |
Protective Coating PC-Wood Guardian™ Wood Preservative PC-Wood Guardian™ isused in preventing and controlling decay fungi. It is an effective treatment for wood and wood composite to kill and prevent infestations of decay fungi including white and brow.. |
|||
Bulk Density | >= 0.320 g/cc | >= 0.0116 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical MB802 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Bulk Density | >= 0.320 g/cc | >= 0.0116 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical MB838A Opaque impact modifier Description: MBS type opaque impact modifiers from LG Chem are appropriate for improving impact strength all the PVC products of rigid and semi-rigid opaque PVC, and have differentiated characterist.. |
|||
Bulk Density | >= 0.320 g/cc | >= 0.0116 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical MB885 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1900 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 121 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.320 g/cc | 0.0116 lb/in³ | |
BASF Heligoen® Blue K 6902 Color Additive Chemical Structure: Cu-phthalocyanine alpha stab.Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applica.. |