Polymer Property : Bulk Density = 0.0232 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0190 - 0.0232 g/cc
0.000686 - 0.000838 lb/in³
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Bulk Density 0.0190 - 0.0232 g/cc
0.000686 - 0.000838 lb/in³
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Bulk Density 0.0190 - 0.0232 g/cc
0.000686 - 0.000838 lb/in³
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Bulk Density 0.0190 - 0.0232 g/cc
0.000686 - 0.000838 lb/in³
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..