Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | Loose |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ASTM D4894 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ISO 60 |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ASTM D1895 |
Plenco 6401 Phenolic, Granular, Compression Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | Tap |
TIMCAL TIMREX® T200-2000 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | Vibrated; ASTM D1895 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ASTM D4745 |
3M Dyneon™ CC605 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 25% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |